Dhexroorka | Culayska Xoojinta | Xoog xajin | Xoog xiirid | E-modulus(GPa) |
6 | 38 | 1300 |
≥150 |
≥55 |
12 | 125 | 1200 | ||
16 | 185 | 1000 | ||
20 | 255 | 900 | ||
25 | 410 | 850 |
Dhexroor badan sida shuruudaha
Magaca | BFRP Rebar | |
Cufnaanta (g/cm³) | 1.9 ~ 2.1 | |
Xoogga Jilitaanka (MPa) | ≥750 | |
Tensile M-modulus(MPa) | ≥4.0 | |
Dheeraynta(%) | ≥1.8 | |
Kulul isku xidhka ballaarinta (×10+/℃) | Dheeraad ah | 9 ~ 12 |
| Horizontal | 21 ~ 22 |
E Iska caabinta Alkali (Xoojinta Haysashada %) | ≥85 | |
U nugulnaanta birta (4 π x10 SI) | ≤5 |
Dock, Biyo-xireenka, taageerada wadada macdanta, dhismaha xoojinta. Xoojinta buundada wadada la taaban karo
NMR/CT dhismayaasha, isbitaalada
Rxoojinta fiilooyinka indhaha iyo xargaha xargaha, Taawarrada Isgaarsiinta Telefishinka
IYOsaldhigyada korantada